钢厂
退火温度对3.1%Si无取向硅钢组织织构与磁性能的影响
研究了退火温度对3.1%Si无取向硅钢组织和磁性能的影响规律。结果表明:退火温度从940℃提高至1 000℃,平均晶粒尺寸由98μm增加到145μm,铁损P1.5/50从2.576 W/kg降低至2.408W/kg。随着退火温度的升高,γ不利织构组分强度逐渐降低,{111}〈112〉织构组分强度降低约16%,磁感B50逐渐升高,磁性能水平提高。 The effects of annealing temperature on microstructure and texture and magnetic properties of 3.1%Si non-oriented silicon steel were investigated in this paper.The results showed that,when the annealing temperature increased from 940℃ to 1 000℃,the average grain size of metallographic structure increased from 98μm to 145μm,the iron loss value P1.5/50 decreased from2.576 W/kg to 2.408 W/kg.And as the annealing temperature increased,the strength of the unfavorable texture componentγgrad...
CSP工艺生产无取向电工钢
介绍了CSP工艺生产无取向电工钢各工序的设备特点、采用的工艺控制手段和电工钢产品质量情况,结合生产实践证明了马钢CSP工艺开发的无取向电工钢产品丰富了薄板坯连铸连轧的品种结构,发挥了薄板坯连铸连轧生产无取向电工钢性能均一、稳定的特点。 The equipment characteristic,the process control method and the quality of non-orientated silicon steel by CSP process were introduced.Combined with the production situation,it is proved that production of non-orientated silicon steel developed on Masteel CSP line would enrich product structure of thin slab continuous casting and rolling,and it exerts stable performance of non-orientated silicon steel.
辉光放电发射光谱法测定硅钢薄板中微量硼元素
通过对辉光放电发射光谱参数的优化,以铁元素为内标来消除基体效应,建立了测定硅钢薄板中微量硼元素的方法。优化的实验参数为:放电电压1200 V,放电电流50 mA,预溅射时间40 s,积分时间10 s。校准曲线硼元素含量范围0.0001%~0.022%,相关系数大于0.999,测量结果与认定值一致,相对标准偏差小于10%。完全能够满足日常分析测试的要求。 A glow discharge optical emission spectrometry(GD-OES) method for determining trace boron element in silicon steel sheets were established through optimization of instrumental parameters and using Fe element as an internal standard to eliminate the matrix effect.The optimized instrumental parameters included discharge voltage,discharge current,pre-sputtering time and integration time,which are 1200 V,50 mA,40 s,and 10 s,respectively.The content of boron element that can be determined from the ca...
常化温度对含1.5%Si无取向电工钢磁性能的影响
研究了CSP工艺流程生产的硅含量为1.5%的无取向电工钢在不同常化温度下对磁性能的变化。研究结果表明:随着常化温度的提高,热轧板的晶粒尺寸增大,且组织均匀性提高;此外成品的有利织构组分{100}<0vw>、α、η增强,不利织构组分减弱;铁损P1.5/50呈下降趋势,磁感B50上升平缓。在常化工艺为970℃×2.5min下,对应的铁损P1.5/50<3.4W/kg,磁感B50>1.74T。 The effect of normalizing temperature on the magnetic properties of non-oriented electrical steel containing 1.5%silicon produced by CSP process was studied.The results show that with increasing normalizing temperature,the average grain size of hot-rolled plate increases and the microstructure uniformity is improved.Furthermore,the texture components of finished products are improved through enhancing of{100}<0vw>,αandηtextures and weakening of{111}<112>texture;the core loss P1.5/50 ...
高牌号无取向电工钢技术发展及应用
对高牌号无取向电工钢国内生产情况、工艺技术、产品性能及应用领域等进行了阐述,并探讨了高牌号无取向电工钢产品的发展趋势。 This paper introduces basic facts on the production status,process technology and products’ properties and their applications of non-oriented electrical steel with high grade at home,and then discusses the development trend on technology for producing the non-oriented electrical steel with high grade.
常化对含硅1.6%的无取向电工钢组织和织构的影响
研究了常化对CSP流程生产的wSi=1.6%的无取向电工钢组织、织构和成品磁性能的影响。结果表明,经CSP流程生产,且在相同的冷轧及退火制度下,经1 000℃×2min常化处理的wSi=1.6%的无取向电工钢热轧板,其最终退火成品的铁损P15/50比不常化试样下降了10.5%,磁感B50比不常化试样提高了2.5%;常化使wSi=1.6%的无取向电工钢成品的平均晶粒尺寸增大,成品铁损P15/50相应减小;同时,常化使wSi=1.6%的无取向电工钢成品中高斯织构的强度增加,γ纤维织构的强度减弱,这有利于成品磁感B50的提高。 The effect of normalizing on microstructure,texture and magnetic properties of non-oriented electrical steel with wSi=1.6% produced by CSP process was investigated.The results show that,under the same cold rolling and annealing system,the iron loss(P15/50) of annealed samples whose hot bands has been normalized by 1 000 ℃×2 min process decreases by 10.5% and magnetic induction(B50) increases by 2.5% compared with the samples whose hot bands was not normalized.The average grain size of non-orient...
无取向硅钢钢液增钛原因分析
对无取向硅钢炼钢全流程钢液增钛的原因进行了分析,认为铁水钛含量、转炉出钢温度、转炉下渣量、精炼渣TiO2含量、钢水罐及RH浸入管混钢种生产是影响钢液增钛的主要原因。通过采取低钛铁水冶炼,减少转炉下渣量,提高出钢温度,添加白灰改质精炼渣等措施,均能够降低钢液中的钛含量。 After analyzing the causes leading to increased content of titanium in molten nonoriented silicon steel during whole steelmaking process, it was concluded that such factors as content of titanium in hot metal, tapping temperature from converter, quantity of roughing slag entered into the ladle from converter, content of TiO2 in refining slag, molten steel ladle car,carrying out the steelmaking of different steel grades by the same ladle and same RH immersion tube were the main causes ...
硅钢在连续退火机组浪形缺陷的控制
为了消除硅钢在连续退火机组产生的浪形缺陷,对浪形缺陷产生的主要原因进行了分析。制定了相应控制措施,对炉内带钢张力、冷却段输出、碳套辊与带钢的同步性、无氧化炉燃烧状态等参数进行了调整;在生产组织上安排高低牌号宽窄规格穿插生产、定期更换碳套辊等,实施后效果明显。 The main cause leading to waviness defects of silicon steel is analyzed in order to eliminate the waviness defects of silicon steel in continuous annealing line.And thus corresponding measures for controlling these defects are made by means of adjusting these parameters such as the tension of silicon steel coils in continuous annealing furnace,the output in cooling section and the combusting condition of the non-oxidation furnace as well as keeping the synchronization between carbon sleeved roll...
热轧工艺对TSCR流程生产取向硅钢组织和性能的影响
取向硅钢热轧板中组织、织构梯度对发展完善的二次再结晶十分关键,通过对2种不同热轧工艺生产取向硅钢的组织、织构进行研究,结果表明:采用后道次大压下热轧工艺时热轧板表层再结区晶粒平均尺寸增加,再结晶区厚度增加,高温退火后二次晶粒尺寸减小;采用后道次大压下热轧工艺热轧时,热轧板中平均等效应变高,热轧板厚度心部{100}〈011〉和{100}〈001〉位向取向强度降低,({111}~{113})〈110〉位向取向强度提高,高温退火后{110}〈001〉位向偏离角降低,磁性能提高。 The texture and microstructure gradient in hot rolled grain oriented silicon steel strip was one of the essential factors to achieve a perfect secondary recrystallization.The texture and microstructure of grain oriented silicon steel strip as-rolled with two different hot rolling parameters was investigated.The results show that with big reduction at the end rolling process,the intensity of {100}〈011〉 and {100}〈001〉 orientation reduces with({111}-{113})〈110〉 orientation intensity enhanced in hot...
CSP流程热轧板常化温度对冷轧无取向电工钢退火组织和磁性能的影响
研究了CSP工艺生产≤0.005%C-1.1%Si的2.2mm无取向电工钢热轧板在800~1000℃常化对0.5mm冷轧板840℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感增加;热轧板常化温度超过900℃,因第二相固溶而后弥散析出,退火后冷轧晶粒细化,铁损增加,因此该无取向电工钢热轧板最佳常化温度为900℃。 The effect of normalizing at 800-1000℃ of CSP produced plate(≤0.005%C-1.1%Si) on the microstructure and magnetic properties of downstream cold-rolled non-oriented electrical steel annealed at 840℃ was studied.Results show that with increasing normalizing temperature of hot-rolled material the recrystallized grain size of annealed sheet increases,iron loss reduced and magnetic induction increases.As normalizing temperature excesses 900℃,grain is refined and iron loss increases after annealing due...