  • 未分类

取向硅钢热轧板中组织、织构梯度对发展完善的二次再结晶十分关键,通过对2种不同热轧工艺生产取向硅钢的组织、织构进行研究,结果表明:采用后道次大压下热轧工艺时热轧板表层再结区晶粒平均尺寸增加,再结晶区厚度增加,高温退火后二次晶粒尺寸减小;采用后道次大压下热轧工艺热轧时,热轧板中平均等效应变高,热轧板厚度心部{100}〈011〉和{100}〈001〉位向取向强度降低,({111}~{113})〈110〉位向取向强度提高,高温退火后{110}〈001〉位向偏离角降低,磁性能提高。 The texture and microstructure gradient in hot rolled grain oriented silicon steel strip was one of the essential factors to achieve a perfect secondary recrystallization.The texture and microstructure of grain oriented silicon steel strip as-rolled with two different hot rolling parameters was investigated.The results show that with big reduction at the end rolling process,the intensity of {100}〈011〉 and {100}〈001〉 orientation reduces with({111}-{113})〈110〉 orientation intensity enhanced in hot... 
2012-12-28 624 5.8

利用场发射电镜及能谱仪研究了取向电工钢薄、厚板坯铸锭中不同区域的析出相差异,确定了MnS、AlN及Fe3C的析出顺序和形貌特征。结果表明AlN以先析出的MnS为形核核心,形成粗大微米级的复合析出相。针状Fe3C既可以在复合析出相表面形成也可以在基体中单独出现,主要受冷却速度的影响。在1250℃保温1~2 h,AlN、Fe3C均可完全回溶,但部分MnS仍不回溶。MnS尺寸随着保温时间延长而增大。导致热轧板中沿轧向分布的粗大MnS,减弱了粒子钉扎力。 Precipitates in thin and thick slabs of electrical silicon steel were investigated by means of field emission SEM and EDS analysis.The precipitation sequence and the morphology of MnS,AlN and Fe3C particles were identified.AlN particles are observed to be nucleated on surface of MnS forming micron-meter-sized complex particles.Acicular Fe3C can precipitate on surface of the complex MnS/AlN particles or directly from matrix depending on cooling rate of the slabs.After holding at 1250 ℃ for 1-2 h,... 
2011-08-28 211 5.8

研究了常化对CSP流程生产的wSi=1.6%的无取向电工钢组织、织构和成品磁性能的影响。结果表明,经CSP流程生产,且在相同的冷轧及退火制度下,经1 000℃×2min常化处理的wSi=1.6%的无取向电工钢热轧板,其最终退火成品的铁损P15/50比不常化试样下降了10.5%,磁感B50比不常化试样提高了2.5%;常化使wSi=1.6%的无取向电工钢成品的平均晶粒尺寸增大,成品铁损P15/50相应减小;同时,常化使wSi=1.6%的无取向电工钢成品中高斯织构的强度增加,γ纤维织构的强度减弱,这有利于成品磁感B50的提高。 The effect of normalizing on microstructure,texture and magnetic properties of non-oriented electrical steel with wSi=1.6% produced by CSP process was investigated.The results show that,under the same cold rolling and annealing system,the iron loss(P15/50) of annealed samples whose hot bands has been normalized by 1 000 ℃×2 min process decreases by 10.5% and magnetic induction(B50) increases by 2.5% compared with the samples whose hot bands was not normalized.The average grain size of non-orient... 
2012-11-28 222 5.8

通过对辉光放电发射光谱法分析电工钢样品光谱行为的研究,分析其工作参数如:电压、电流、预溅射时间和积分时间对光谱强度和稳定性的影响,并以铁为内标元素,优化了工作参数。确定了直流辉光放电光谱法测定电工钢中碳、硅、锰、磷、硫、铬、镍、铜共8种元素的定量分析方法,并对该方法分析的精密度和准确度进行验证,结果表明,各元素的测定结果与认定值和其他方法测定值一致,测量元素结果RSD值小于2%。 Based on research on analyzing the spectrum behavior of the sample taken from the electrical steel by glow discharge optical emission spectrometry,the effect of its operational parameters such as current,voltage,pre-sputtering time and integrating time on the spectral intensity and spectral stability is analyzed.Taking the Fe as an element applied by internal standard method,these operational parameters are optimized,and therefore the quantitative analysis method for testing eight kinds of eleme... 
2011-01-28 220 5.8

研究了CSP工艺生产≤0.005%C-1.1%Si的2.2mm无取向电工钢热轧板在800~1000℃常化对0.5mm冷轧板840℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感增加;热轧板常化温度超过900℃,因第二相固溶而后弥散析出,退火后冷轧晶粒细化,铁损增加,因此该无取向电工钢热轧板最佳常化温度为900℃。 The effect of normalizing at 800-1000℃ of CSP produced plate(≤0.005%C-1.1%Si) on the microstructure and magnetic properties of downstream cold-rolled non-oriented electrical steel annealed at 840℃ was studied.Results show that with increasing normalizing temperature of hot-rolled material the recrystallized grain size of annealed sheet increases,iron loss reduced and magnetic induction increases.As normalizing temperature excesses 900℃,grain is refined and iron loss increases after annealing due... 
2012-03-28 194 5.8

本文以热轧常化板为初始材料,采用二次冷轧法与三次冷轧法制备了0.1 mm厚的取向硅钢薄带,测定相应的磁性能,并通过EBSD取向成像技术检测了二次冷轧法与三次冷轧法各工艺过程中织构与组织演变规律。结果表明,采用最终冷轧压下率适中的三次冷轧法,能在冷轧至0.1 mm时保存较多的高斯晶核,使得高温退火后的磁性能明显优于二次冷轧法。最终冷轧压下率通过影响脱碳退火后样品中的{111}<112>织构组分及Goss晶粒数量对最终二次再结晶产生重要影响。 Grain-oriented silicon steel sheets with a thickness of 0. 1 mm were produced from hot-rolled and normalized sheets by two-step-rolling and three-step-rolling methods. Their magnetic properties were measured,and the textures were detected by EBSD technique. The results show that the three-step-rolling method,which has a moderate reduction rate of final cold rolling,can maintain more { 110} < 001 >nucleus,and thus obtaining better magnetic properties compared with the two-step-method. The f... 
2013-04-28 297 5.8

结合冶炼无取向硅钢的生产实际,对钢中硫的来源,以及炉渣性质、钢水温度、底吹强度对脱硫的影响进行了分析。研究表明,转炉钢中硫的主要来源为铁水、废钢、铁水渣及石灰带入;冶炼硅钢时,终渣碱度为3.0~3.5,w((FeO))≤20%,终点钢水温度大于等于1 680℃,加大底吹搅拌强度能提高转炉脱硫效果。硅钢平均出钢硫的质量分数为0.004 8%,能满足无取向硅钢对硫含量的要求。 With the actual production of non-oriented silicon steel,the source of sulphur and the effect of metallugic parameters like slag properties,temperature of molten steel and bottom stirring on desulphurizing ability were investigated.The results show that the main source of sulphur is molten metal,scrap,the remaining slag volume in hot metal and lime.The degree of desulphurization for smelting silicon steel can be increased through adopting the following measures,such as the basicity of finishing ... 
2011-02-28 279 5.8

针对马钢无取向电工钢孔洞缺陷的分布规律及形貌特征,对缺陷样进行了显微分析,并利用生产实绩数据分析了该缺陷产生的原因。结合热轧生产过程,主要通过避免带钢撞击导卫以及降低导卫结瘤的产生等措施,可有效抑制热卷异物压入产生,从而降低冷轧工序孔洞的产生。 In viewing of the distribution and morphology characteristics of the hole defect of non-oriented electrical steel in Maanshan Iron and Steel Co.,Ltd.,the causes of the defect were analyzed by micro analysis of the defect sample and the production data.Combined with the production process of hot rolling,by avoiding the impact of strip steel on the guide and reducing the nodule formation on the guide,the pressing of foreign bodies in hot coiling could be effectively suppressed,thus reducing the fo... 
2022-01-28 218 5.8

【作者】 王磊; ...
2014-06-28 181 5.8

【作者】 朱凤泉; 黄生银; ...
2013-01-28 230 5.8

为了消除硅钢在连续退火机组产生的浪形缺陷,对浪形缺陷产生的主要原因进行了分析。制定了相应控制措施,对炉内带钢张力、冷却段输出、碳套辊与带钢的同步性、无氧化炉燃烧状态等参数进行了调整;在生产组织上安排高低牌号宽窄规格穿插生产、定期更换碳套辊等,实施后效果明显。 The main cause leading to waviness defects of silicon steel is analyzed in order to eliminate the waviness defects of silicon steel in continuous annealing line.And thus corresponding measures for controlling these defects are made by means of adjusting these parameters such as the tension of silicon steel coils in continuous annealing furnace,the output in cooling section and the combusting condition of the non-oxidation furnace as well as keeping the synchronization between carbon sleeved roll... 
2013-03-28 195 5.8

根据新日铁、JFE及浦项等国外钢铁公司2008年以来在日本专利局、欧洲专利局(EP)及世界知识产权组织(WIPO)申请公开的有关生产Hi-B取向电工钢典型专利技术,概述了近年来国外大型钢铁企业采用低温板坯加热(坯加热温度<1 280℃)技术生产Hi-B取向电工钢主要技术重点,即将调节关键化学成分Al、N、Sn及Sb等与工艺改进相结合。最后介绍了国外大型钢铁企业采用低温板坯加热技术生产Hi-B取向电工钢实例。 The latest developments on technology for manufacturing Hi-B grain oriented electrical steel sheets developed by Nippon Steel Corp.,JFE Steel and POSCO were described according to the patents published by World Intellectual Property Organization,Japan Patent Office and European Patent Office over the recent years.The low temperature slab heating process(particularly slab-heating temperature<1 280 ℃) together with suitably adjusting key chemical elements such as Al,N,Sn and Sb elements was the... 
2013-03-28 334 5.8