针对马钢无取向电工钢孔洞缺陷的分布规律及形貌特征,对缺陷样进行了显微分析,并利用生产实绩数据分析了该缺陷产生的原因。结合热轧生产过程,主要通过避免带钢撞击导卫以及降低导卫结瘤的产生等措施,可有效抑制热卷异物压入产生,从而降低冷轧工序孔洞的产生。 In viewing of the distribution and morphology characteristics of the hole defect of non-oriented electrical steel in Maanshan Iron and Steel Co.,Ltd.,the causes of the defect were analyzed by micro analysis of the defect sample and the production data.Combined with the production process of hot rolling,by avoiding the impact of strip steel on the guide and reducing the nodule formation on the guide,the pressing of foreign bodies in hot coiling could be effectively suppressed,thus reducing the fo... 
2022-01-28 218 5.8

对冷轧无取向硅钢在冶炼过程中各个工序的顶渣进行了检测,分析了顶渣变化原因,并得出结论:硅钢生产宜采用复吹转炉,以降低吹炼终点渣中TFe含量,进而减轻对精炼的压力;使用低S、低Al2O3含量中间包覆盖剂;RH脱氧及合金化顺序采用先加硅铁后加铝;首罐宜经LF提温并降低渣中TFe。 The top-surface slag used for the various production processes in smelting coldrolled non-oriented electrical steel is tested and based on tested results the cause of the top surface slag change is analyzed.So it is concluded that the combined blown converter is more suitable to be used for smelting electrical steel in order to reduce the content of TFe in slag at blow end point and then much better results can be achieved during the period of refining.Secondly the tundish flux contenting low co... 
2013-03-28 204 5.8

研究了采用高温卷取热轧态原料和常化态原料生产高牌号冷轧无取向电工钢组织、织构和磁性能。研究发现钢卷采用750℃高温卷取,下线后立即采用\"保温罩\"对钢卷进行保温,时间96h,然后空冷至100℃时上线生产的工艺可取代常化工艺生产高牌号冷轧无取向电工钢。冷轧上线前,热轧态原料的表层为大量的再结晶组织,这部分组织包括了热轧轧制时保留下来的动态再结晶组织,钢卷本身高温回复后产生再结晶晶粒,以及在保温罩内保温时形成的再结晶组织。高温卷取的热轧态和常化态的热轧卷作为原料时,试样织构类型相似,取向分布密度接近,再结晶后织构类型仍然相似,取向分布密度仍然接近。Goss织构对磁性能增加有促进作用。实验钢中较好的磁性能对应的织构[{100}+Goss]/{111}的比值较高,体现了织构的遗传性。 Microstructure,texture and magnetic properties of high grade cold rolled nonoriented electrical steel which made of hot rolled material with high temperature coiling and with normalization were studied.Steels coiled in high temperature(at 750 ℃),stacked with insulation cover for 96hand air cooled to 100 ℃ were using to manufacture high grade nonoriented electrical steel.The process can replace the normalization process.There are a lot of recrystallized grains in the surface layer of the coil wit... 
2014-03-28 215 5.8

冷轧中中低牌号的无取向硅钢多采用万能凸度轧机(Universal crown mill,UCM)生产,其板形好坏受制于UCM轧机板形调节手段的协调使用。为掌握UCM轧机的板形控制特点,建立基于二维变厚度有限元的辊系弹性变形和基于三维差分的轧件塑性变形的六辊轧机耦合模型,对UCM轧机的板形调控性能进行详尽的分析,包括工作辊和中间辊弯辊、中间辊窜辊的调控功效、辊间接触压力分布等。在此基础上,提出可用指导生产的板形控制策略,指出UCM轧机在横向厚差控制方面的不足。针对工业生产中UCM轧机轧制无取向硅钢横向厚差大的问题,在大量仿真计算的基础上,开发具有高次曲线函数的边部变凸度(Edge variable crown,EVC)的工作辊。采用该工作辊后,各种品种的无取向硅钢的横向厚差不大于10μm的百分比由24%提高到99%,横向厚差的均值小于6μm,远小于之前的13μm。 Medium-low grade non-oriented silicon steel is rolled often by universal crown mill(UCM) during cold rolling.Its shape quality is dependent on the coordinated control of several shape adjustment devices of UCM.In order to understand the shape control characteristics of UCM,coupling model of six-high rolling mill,based on two-dimensional varying thickness finite element rolls elastic deformation model and three-dimensional finite difference strip plastic deformation model,is setup for the detaile... 
2011-10-28 207 5.8

本文以热轧常化板为初始材料,采用二次冷轧法与三次冷轧法制备了0.1 mm厚的取向硅钢薄带,测定相应的磁性能,并通过EBSD取向成像技术检测了二次冷轧法与三次冷轧法各工艺过程中织构与组织演变规律。结果表明,采用最终冷轧压下率适中的三次冷轧法,能在冷轧至0.1 mm时保存较多的高斯晶核,使得高温退火后的磁性能明显优于二次冷轧法。最终冷轧压下率通过影响脱碳退火后样品中的{111}<112>织构组分及Goss晶粒数量对最终二次再结晶产生重要影响。 Grain-oriented silicon steel sheets with a thickness of 0. 1 mm were produced from hot-rolled and normalized sheets by two-step-rolling and three-step-rolling methods. Their magnetic properties were measured,and the textures were detected by EBSD technique. The results show that the three-step-rolling method,which has a moderate reduction rate of final cold rolling,can maintain more { 110} < 001 >nucleus,and thus obtaining better magnetic properties compared with the two-step-method. The f... 
2013-04-28 297 5.8

对CSP流程生产的高磁感无取向电工钢50W1300在偏离轧制方向不同角度处的磁性能进行了测试和分析。结果表明:在偏离轧向不同角度处,磁性能差异显著,尤其在α=60°时磁感最低;偏离轧制方向不同角度处的磁性能大小取决于织构类型、强度及分布状态;增强{100}<0vw>和α、η取向的有利织构组分,降低不利的γ取向织构组分,且使有利织构组分分布越漫散,磁各向异性越小。 Magnetic properties of high magnetic induction non-oriented electrical steel 50W1300 produced by CSP processes were investigated with different direction in relation to the rolling direction.The result shows that magnetic properties are significantly different in relation to the rolling direction,in particular,the minimum magnetic induction occurs at 60° in relation to the rolling direction.Magnetic properties of different directions in relation to rolling direction depend on type and distributi... 
2011-04-28 393 5.8

对高牌号无取向电工钢35W300的成品进行了第二次退火,对第二次退火后的成品性能、纵横向磁性能差异和组织变化进行了分析。结果表明,随着第二次退火温度的升高,晶粒长大,磁性能优化。铁损平均值下降0.087 5W/kg,磁感平均值升高0.008T。第二次退火温度为820℃的产品的磁性能能够满足用户使用要求。 The product of high grade non-oriented electrical steel 35W300 was annealed at the second time.Microstructure,the difference of magnetic properties in the vertical and horizontal and were studied.The results show that the grain grew up and magnetic properties optimized with the increase of annealing temperature for the second time.Iron loss average declines in 0.0875 W/kg,magnetic induction average increases 0.008 T.The magnetic properties can meet the requirements of users at the second anneali... 
2013-04-28 385 5.8

【作者】 卢鹏; ...
2013-03-28 438 5.8

研究了CSP工艺生产≤0.005%C-1.1%Si的2.2mm无取向电工钢热轧板在800~1000℃常化对0.5mm冷轧板840℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感增加;热轧板常化温度超过900℃,因第二相固溶而后弥散析出,退火后冷轧晶粒细化,铁损增加,因此该无取向电工钢热轧板最佳常化温度为900℃。 The effect of normalizing at 800-1000℃ of CSP produced plate(≤0.005%C-1.1%Si) on the microstructure and magnetic properties of downstream cold-rolled non-oriented electrical steel annealed at 840℃ was studied.Results show that with increasing normalizing temperature of hot-rolled material the recrystallized grain size of annealed sheet increases,iron loss reduced and magnetic induction increases.As normalizing temperature excesses 900℃,grain is refined and iron loss increases after annealing due... 
2012-03-28 194 5.8

通过对辉光放电发射光谱法分析电工钢样品光谱行为的研究,分析其工作参数如:电压、电流、预溅射时间和积分时间对光谱强度和稳定性的影响,并以铁为内标元素,优化了工作参数。确定了直流辉光放电光谱法测定电工钢中碳、硅、锰、磷、硫、铬、镍、铜共8种元素的定量分析方法,并对该方法分析的精密度和准确度进行验证,结果表明,各元素的测定结果与认定值和其他方法测定值一致,测量元素结果RSD值小于2%。 Based on research on analyzing the spectrum behavior of the sample taken from the electrical steel by glow discharge optical emission spectrometry,the effect of its operational parameters such as current,voltage,pre-sputtering time and integrating time on the spectral intensity and spectral stability is analyzed.Taking the Fe as an element applied by internal standard method,these operational parameters are optimized,and therefore the quantitative analysis method for testing eight kinds of eleme... 
2011-01-28 220 5.8

利用场发射电镜及能谱仪研究了取向电工钢薄、厚板坯铸锭中不同区域的析出相差异,确定了MnS、AlN及Fe3C的析出顺序和形貌特征。结果表明AlN以先析出的MnS为形核核心,形成粗大微米级的复合析出相。针状Fe3C既可以在复合析出相表面形成也可以在基体中单独出现,主要受冷却速度的影响。在1250℃保温1~2 h,AlN、Fe3C均可完全回溶,但部分MnS仍不回溶。MnS尺寸随着保温时间延长而增大。导致热轧板中沿轧向分布的粗大MnS,减弱了粒子钉扎力。 Precipitates in thin and thick slabs of electrical silicon steel were investigated by means of field emission SEM and EDS analysis.The precipitation sequence and the morphology of MnS,AlN and Fe3C particles were identified.AlN particles are observed to be nucleated on surface of MnS forming micron-meter-sized complex particles.Acicular Fe3C can precipitate on surface of the complex MnS/AlN particles or directly from matrix depending on cooling rate of the slabs.After holding at 1250 ℃ for 1-2 h,... 
2011-08-28 211 5.8

【作者】 王磊; ...